Originally Posted by talcum
No - I mean self assembled nanotubes using a mask and PMMA like the big boys.

My issue seems to be that we're talking 10-50 nanometers for the tube using self assembly and more for a mask like that used for the wafer.

Maybe I can try something at this end.

-talc

Nanometers? We're still dealing with hundreds of microns here.

Big boys? Sorry, doing what I can on a budget that amounts to around $1500 US max.

Happy to know if there's some way to do things better though.