tough to get a good o-ring channel with a drill press
Won't need an O-Ring. RTV silicone will work fine. Been using it for years on blocks and has yet to fail. In fact the barbs on the Lumpy Channel blocks pH tested were sealed with clear RTV silicone. Or being it is all copper one can solder it if they feel up to it.

The R-Type also has a thicker base and the pins are taller than the channels on the LC. The thicker base made most of the difference I belive. I am going to make a modified LC with a thicker base and taller channels and send it to pH sooner or later to back this up.