Quote:
Originally Posted by G33k
kbn : Just to satisfy my curiosity, would I be right in thinking annealing is used to soften a metal? If that's the case, why would you want to soften an already fairly soft (compared to say steel) metal? *senses interesting project*
For my hdd cooler (see the hdd thread) I needed to bend copper sheet around copper pipe and as i dont have the proper tools for doing it I need it to be as soft as possible.

When the copper went red it was sorta a darkish red and I could see it easly but my dad had to turn the light off to see it (slightly colour blind), I think I could have got it hotter but not much, the copper was in the middle of the flame.
|kbn| is offline   Reply With Quote