Quote:
Had made the switch to machining with Delrin 3 months ago. Yeah - about $5 difference. Agree with its wonderful properites.
True for waterblock tops, but to my understanding, a pump is a lot more machining and material. Is it true for this as well? This is a budget pump while your stuff is high end waterblocks, so does the "value" of $5 change?

Is anodizing the only solution to dealing with corrosion? What about nickel or gold plating? Would that work as well/better?