Originally Posted by SysCrusher
Brass is going to add some weight to it so keep that in mind. Another option is delrin.
and delrin cant crack?

Quote:
Originally Posted by killernoodle
UHMW polyethylene (sp?) is good for waterblocks: it is easy to machine, it is does not absorb water at all, it is scratch resistant, and looks very nice on a block. Plus when you screw barbs in, it stretches slightly and can nearly florm a perfect seal by itself.
the same here.

There are an other problem when milling plastic, they flex = the size is not the same when U have fixed it in the mill.