Thanks for the info Dave.

Quote:
Why did we never cut the pump housing of the 750 out of solid Delrin? Not sure, I'll ask, but I suspect Dan likely didn't see a reason for it, as we have never seen a pump fail because of pitting. Remember there is a big difference between galvanic corrosion and natural oxidation. I plan on making a Delrin MAG rear case later this week to see how it looks thanks to a suggestion on this board.
I'm sure there's a logical reason why AL was used for the pump housing, but am not clear why Delrin wasn't used for the threaded pump head.

yes pls let us know how the Delrin turns out on the new MAG pumps