Quote:
Originally Posted by killernoodle
According to the JB weld's resin's MSDS, it contains 10-20% iron (why isnt it conductive?)

I dunno, you could try adding copper dust or something like that in with it.

Actually, that is kinda what I will be doing, but using a something besides copper dust. J B Weld will only make up about 5% - 10% of mass.

MaxSaleen, I'm trying to tie several heat sources into one common tim that must be formable. Not trying to be secretive, just a project I'm working on...