Thats only for metal though..?

Most joints are brass-to-polycarb or acylic.

Ill be using BSPP parrelell barbs in future as they are more reliable than taper threads when used on plastics. They dont leak when tightend properly and can be overtightend a bit without risk of cracking the plastic.

All metal-metal joints in my system are soldered, becuase its a lot easyer, stronger, and reliable than any sealant could be.


The circuit would cost almost nothing, which is why Im tempted to make it although I agree it is not really needed, and having the extra wires round my case would probably annoy me more than having lots of slow leaks...