Quote:
Originally posted by Pyrotechnic
I'll be the lab rat this time. I got a gallon of coolant i mixed up and only 1/2 of it used. It consists of about %70 Distilled waster and %30 Prestone ethylene glycol antifreeze. i got a piece of copper flat bar and a big all alluminum non - anodized PII heatsink. I'll put these in the coolant for a week or so and see what i get. I have been running this coolant in my system for 2 days now and see no problems, my system is all copper by the way.
|
your mixture is not what we have been doing. the glycol is more for low temps... not designed to stop corrosion... the redline and purpleice are more of an additive.. not a large part of the mixture... BUT im sure you all know this... and i wanna see what the corrosion results are with this... hrmmm =)
oh.. the distilled water is still showing no signs of corrosion... but there is a decent ammount on a straight tap mixture i made about 3 days into the test.. lots of white furry stuff on the aluminum