Quote:
Originally posted by MeltMan
Whats the problem? Im not talking about the interface side of anything here... I'm talking about the top, and the sides of the block. Who gives a crap if the top and sides are microscopically concave or convex? Point is, you cant tell by looking at it and it achieves a better finish than lapping alone.

Polishing with arctic silver is pointless. Its not an abrasive, its a thermal interface material. The only thing I can see this helping is if you rub some into your lapped side (CPU side) to kind of "prime" the copper for its actual interface.
Sorry, I WAS talking about lapping the block.

A buffing wheel would indeed work quite nicely, as you demonstrate every day! I've used mine to buff glass, and it works great. It's trickier to do on plastics...
bigben2k is offline   Reply With Quote