I think you can tell by this pic that the edges were in contact with the center with just a little sanding on the left. Even after further sanding the same amount was removed frof the edges as in the middle. The pic on the right shows the copper exposed in the center and the edges but the plating is still on the belly and that is how I left it (good thing too). Some creative sanding by me will remove some more from the edges alone to get some central presure for the way it was designed to be. Thanks for the info BillA.
Attached Images
File Type: jpg ihs_lapping.jpg (10.3 KB, 72 views)
gone_fishin is offline   Reply With Quote