Neomoses or cathar i have a quick question for either of you. as per a previous thread i have an abundance of aluminum to play with and use along with the tooling to play with blocks and (test isn't the right word but the only one i can think of here) test different designs also. I came up with a similar drawing in cad after thinking about the leamonblock design, but believe this might be better. to make the slots i have a great end mill saw that you can setup to slot very fine channels in materials. my question is if someone were to do it similar on a base plate as you had with your copper about what bp thickness would you start with to try it out in al?