Hey one more little trick that I discovered while brazing my waterblock together... If you want to have some control over where the solder bonds, try coating a side with PERM marker (Sharpie) and it'll smoke a little till it's solvent free, but watch as the brazing material magically stays unbonded to the perm-marker side! Works really well for controlling flow of the solder and can removed with alcohol or some other solvent.... Remember EYE protection!